Causes of cracks in cast iron castings

Time:2021-11-25 09:58:25 Author:Daguang JinpengClick:60

Causes of cracks in cast iron castings

Cracks(hot cracks,cold cracks)

Features:the crack appearance is straight or irregular curve,the hot crack fracture is strongly oxidized to dark gray or black,without metallic luster,and the cold crack fracture is clean and metallic luster.Generally,the external cracks of castings can be seen directly,and the internal cracks can only be seen by other methods.Cracks are usually related to shrinkage cavity,slag inclusion and other defects.Most cracks occur at the inner side of the sharp corner of the casting,the connection between thick section and thin section,and the hot spot between the riser and the casting.

Cause:the metal mold casting is prone to crack defects,because the metal mold itself has no concession and the cooling rate is appropriate,which is easy to increase the internal stress of the casting,open the mold too early or too late,the pouring angle is too small or too large,the coating is too thin,etc.,It is easy to cause casting cracking,and the mold cavity itself is also easy to crack.

Prevention and control methods:

1.Attention shall be paid to the manufacturability of the casting structure.Incoming cast iron parts shall make the transition of parts with uneven wall thickness uniform,and appropriate fillet size shall be adopted.

2.Adjust the coating thickness to make each part of the casting reach the required cooling rate as much as possible to avoid excessive internal stress.

3.Pay attention to the working temperature of the metal mold,adjust the inclination of the mold,timely pull out the core and cracks,and take out the casting for slow cooling.

Features:cold shut is a kind of surface crack with through seam or round edge.The middle of the cast iron model is separated by oxide scale,not all of which are integrated.When the cold insulation is serious,it becomes"under cast".Cold insulation often occurs on the top wall of castings,thin horizontal or vertical surfaces,thick thin-walled joints or thin auxiliary plates.

Causes:

1.The exhaust design of metal mold is unreasonable.

2.The working temperature is too low.

3.Poor coating quality(artificial and material).

4.The opening position of runner is inappropriate.

5.Pouring speed is too slow.

Prevention and control methods:

1.Design runner and exhaust system correctly.

2.For large-area thin-wall castings,the factory coating of iron castings should not be too thin.Appropriately thickening the coating is conducive to molding.

3.Properly increase the working temperature of the die.

4.Inclined pouring method is adopted.

5.Mechanical vibration metal mold is used for pouring.

prev:none
next:none